| S.No. | Checkpoint | IS Requirement | Status |
|---|---|---|---|
| A. TEST PROCEDURE | |||
| A1 | DFT (Dry Film Thickness) measured with electronic gauge; typical tolerance ±25 microns Acceptance: Gauge calibrated; substrate and film thickness measured; difference = DFT | Cl. 402 — Measurement method | |
| B. TEST RESULTS | |||
| B1 | Test point 1: DFT measured (microns); location documented Acceptance: Typical spec: 1.5-3.0mm DFT for single/double coat liquid membranes | Cl. 402 — Individual reading | |
| B2 | Test point 2-5: DFT measured at different locations; variations noted Acceptance: 5 test points minimum per 100m²; readings distributed across area; corner/edge samples required | Cl. 402 — Multiple readings | |
| B3 | Average DFT calculated; minimum and maximum values recorded; variation noted Acceptance: Average should meet or exceed spec; variation <±20% from average; consistency indicator | Cl. 402 — Statistical summary | |
| C. ACCEPTANCE CRITERIA | |||
| C1 | DFT compliance: Average measured DFT ≥ specification minimum (typically 1.5mm for single-coat) Acceptance: Single-coat min: 1.5mm; two-coat min: 2.5-3.0mm; all points ≥85% of average acceptable | Cl. 402 — Thickness acceptance | |
| C2 | Uniformity: No point more than ±20% below average; indicates consistent application Acceptance: Variation ≤±20% from average = PASS; >±20% = thin spots requiring re-coat; re-test after touch-up | Cl. 402 — Application quality | |